The defects caused by trapping a gas in molten metal or by mold gases while pouring the melt is known as?

🎲 Try a Random Question  |  Total Questions in Quiz: 20  |  🧠 Study this quiz with Flashcards
This question is part of a full practice quiz:
Manufacturing Engineering Practice Test: Casting Defects / Metal Casting Defects — practice the complete quiz, review flashcards, or try a random question.

A casting defect is an undesired irregularity in a metal casting process. Some defects can be tolerated while others can be repaired, otherwise they must be eliminated.

Casting defects can be broken down into five main categories: gas porosity, shrinkage defects, mould material defects, pouring metal defects, and metallurgical defects.


The defects caused by trapping a gas in molten metal or by mold gases while pouring the melt is known as?