Composition of a Nickel superalloy is as follows: Ni = 70.0%, Cr = 20.0%, Fe = 5.0% and rest Titanium. What will be the rate of dissolution if the area of the tool is 1500 mm2 and a current of 1000 A is being passed through the cell? Assume dissolution to take place at lowest valency of the elements.ANi = 58.71 ρNi = 8.9 νNi = 2ACr = 51.99 ρCr = 7.19 νCr = 2AFe = 55.85 ρFe = 7.86 νFe = 2ATi = 47.9 ρTi = 4.51 νTi = 3

🎲 Try a Random Question  |  Total Questions in Quiz: 65  |  🧠 Study this quiz with Flashcards
This question is part of a full practice quiz:
Manufacturing Engineering Practice Test: Electro-Chemical Grinding Machining — practice the complete quiz, review flashcards, or try a random question.

Electrochemical grinding (ECG) is a machining process that combines electrochemical machining (ECM) and conventional grinding. It's also known as electrolytic grinding or enotic machining. ECG is a non-traditional machining process that uses a negatively charged abrasive grinding wheel, an electrolyte fluid, and a positively charged workpiece to remove electrically conductive material. The workpiece becomes an anode and the grinding wheel becomes a cathode. The process removes material from the workpiece both electrochemically and mechanically. ECG combines electrolytic action (90%) and... Show more

Composition of a Nickel superalloy is as follows: Ni = 70.0%, Cr = 20.0%, Fe = 5.0% and rest Titanium. What will be the rate of dissolution if the area of the tool is 1500 mm2 and a current of 1000 A is being passed through the cell? Assume dissolution to take place at lowest valency of the elements.<br />A<sub>Ni</sub> = 58.71 ρ<sub>Ni</sub> = 8.9 ν<sub>Ni</sub> = 2<br />A<sub>Cr</sub> = 51.99 ρ<sub>Cr</sub> = 7.19 ν<sub>Cr</sub> = 2<br />A<sub>Fe</sub> = 55.85 ρ<sub>Fe</sub> = 7.86 ν<sub>Fe</sub> = 2<br />A<sub>Ti</sub> = 47.9 ρ<sub>Ti</sub> = 4.51 ν<sub>Ti</sub> = 3